Friction Stir Spot Welding: A Review on Joint Macro- and Microstructure, Property, and Process Modelling
Figure 2
Schematic diagram of the refill FSSW process: (a) friction, (b) first extrusion, (c) second extrusion, and (d) pull-out stage [11].