Research Article

Thermal Treatment of Cerium Oxide and Its Properties: Adsorption Ability versus Degradation Efficiency

Figure 4

(a) The Ce 3d peak with deconvoluted components for the sample prepared at the calcination temperature of 200°C. (b) Dependence of the abundances of the Ce 3d components on the calcination temperature.
706041.fig.004a
(a)
706041.fig.004b
(b)