Preparation and Sintering Effect in Quartz-Barium Titanate Porous Ceramics and Permeability Modulation Using an Implanted Electrode
Figure 3
Ceramic digital photographs (10) with scale bar 800 microns for sample with 20% quartz and sintering temperatures of (a) 1200°C, (b) 1000°C, and (c) 800°C.