Review Article

Zeolite Y: Synthesis, Modification, and Properties—A Case Revisited

Figure 12

Degradation of 1 g per L p-chloro-phenol in water by adding of 4 g H2O2 on 10 g of Fenton’s reagent, respectively, zeolite Pt-DAY loaded with 5 mg/g platinum [109].