Research Article

Structural and Morphological Properties of Nanostructured ZnO Particles Grown by Ultrasonic Spray Pyrolysis Method with Horizontal Furnace

Table 1

Variation of crystallite size considering the three most intense diffraction peaks of synthesized ZnO nanoparticles at precursor concentration of 0.01 and 0.1 M, respectively.

Precursor solution concentration(hkl)Crystallite size (nm)
100002101

0.01 M31.753°34.443°36.264°23 ± 4