Research Article
Compressive Fracture of Brittle Geomaterial: Fractal Features of Compression-Induced Fracture Surfaces and Failure Mechanism
Table 1
Total numbers
(
δ) of required cubes and the measurement scales
δ, according to the CCM.
| δ/mm | Tension-induced fracture surfaces | Compression-induced fracture surfaces | No. T-1 | No. T-2 | No. T-3 | No. C-1 | No. C-2 | No. C-3 |
| 0.1 | 11309 | 11197 | 11064 | 10570 | 11294 | 13465 | 0.2 | 2591 | 2575 | 2572 | 2567 | 2579 | 2872 | 0.4 | 628 | 630 | 629 | 634 | 625 | 669 | 0.5 | 401 | 401 | 401 | 404 | 401 | 430 | 1.0 | 100 | 100 | 100 | 100 | 100 | 104 | 2.0 | 25 | 25 | 25 | 25 | 25 | 25 | 2.5 | 16 | 16 | 16 | 16 | 16 | 16 | 5.0 | 4 | 4 | 4 | 4 | 4 | 4 | 10.0 | 1 | 1 | 1 | 1 | 1 | 1 |
|
|