Nanocrystalline 6061 Al Powder Fabricated by Cryogenic Milling and Consolidated via High Frequency Induction Heat Sintering

Figure 7

True stress strain response in simple compression for consolidated samples from the 7 hours cryomilled powders of 6061 AA at the sintering conditions of 500°C–400°C/min–1.5 min at a strain rate of 1 s−1 at room temperature and 200°C.