Research Article

Corrosion Behavior of Pure Cr, Ni, and Fe Exposed to Molten Salts at High Temperature

Figure 1

Micrographs of the cleaned pure chromium, pure nickel, and pure iron after being exposed to NaVO3 for 100 hours at 700°C.