Research Article

Intermetallic Phase on the Interface of Ag-Au-Pd/Al Structure

Figure 4

Observations of bonding interface cross-section featured the following conditions: (a) as-bonded interface at room temperature. Intermetallic compounds were grown for (b) 250 hr, (c) 500 hr, (d) 750 hr, and (e) 1000 hr.
925768.fig.004