Research Article

Reduction of Electromagnetic Interference Using ZnO-PCL Nanocomposites at Microwave Frequency

Table 1

Real and imaginary parts of permittivity for all samples at 8–12 GHz.

Sample Dielectric const.Loss factor

Pure PCL2.790.24
ZnO nano6.481.41
ZnO-PCL-25%ZnO 2.950.27
ZnO-PCL-35%ZnO3.150.39
ZnO-PCL-45%ZnO3.340.46
ZnO-PCL-50%ZnO3.540.50
ZnO-PCL-70%ZnO3.990.63