Evaluation of Permanent Deformation of Unmodified and Rubber-Reinforced SMA Asphalt Mixtures Using Dynamic Creep Test

Table 9

Two-way ANOVA on ultimate strain.

SourceSSdfMS value

Corrected model11575.347 0.000
Intercept112495.6540.000
Stress12203.2680.000
Temperature1779.0590.000
Additive2695.3320.000
Stress temperature1309.4020.000
Stress additive2249.4240.000
Temperature additive2161.8290.000
Stress temperature additive2132.5130.000
Error202728588.943

Total32

a.   Squared = 0.997 (adjusted Squared = 0.995).