Research Article

The Effect of Thermooxidative Aging on the Durability of Glass Fiber-Reinforced Epoxy

Table 1

Changes of curve of EHG250-68-37 composite samples induced by 800 h thermooxidative degradation.

Sample peak (°C) peak area (min)

Unaged115.090.2382
Aged129.720.1927

Area value indicates the area under peak.