Research Article
Mechanism and Durability of Repair Systems in Polymer-Modified Cement Mortars
Table 2
The parameters of polymers.
| | Solid content (%) | Viscosity (mPa·s) | Bulk density (g·cm−3) | pH value | Min film formation temp. (°C) | Glass transition temp. (°C) | Ash content (% by weight) |
| SBR dispersion | 51 | 35–100 | — | 7.8~10 | 15~21 | −3 | — | SAE dispersion | 57 | 50–150 | — | 7.0~8.5 | 1 | −6 | — | SAE powder | — | — | 0.5 | 8.0 | 0 | 15 | 9.5 |
|
|