Research Article

Effect of Curing Temperature Histories on the Compressive Strength Development of High-Strength Concrete

Table 1

Details of concrete mixture proportions.

TypeDesign strength (MPa)W/BUnit weight (kg/m3)
WaterCementSilica fumeSandGravel (%)

I420.415536819.47639730.9
II650.2815552627.77018952.0

= high-range water-reducing agent-to-binder ratio by weight.