Chemical composition of cementitious materials (% by mass).

MaterialsSiO2Al2O3Fe2O3CaOMgOK2ONa2OTiO2SO3

OPC23.303.853.8363.41.241.470.150.332.010.42
SF98.940.300.080.120.040.130.05ā€”0.280.06

Loss on ignition.