Improved Reactivity of Fly Ash-Slag Geopolymer by the Addition of Silica Fume

Table 5

Reactivity of raw material calculated by using NMR deconvolution peaks.

Sample IDFly ash + silica fumeSlagTotal

C57.555.256.3
SF1-1048.445.646.8
SF1-2037.544.942.2
Z1035.681.561.1
HFA44.855.350.0
Z10S43.260.250.8
SF2-1044.272.459.9
SF2-2048.659.155.2
SF2-10S27.282.051.5
SF2-20S24.881.446.0

C and HFA indicate the reactivity of only fly ash.