Research Article

High-Temperature Performance and Multiscale Damage Mechanisms of Hollow Cellulose Fiber-Reinforced Concrete

Table 2

Water absorption ratio of cellulose fibers.

Sample numberDried mass (g)Saturated mass (g)Differential value of mass (g)Water absorption ratio (%)

CF-11.013.442.42240
CF-20.983.312.33238
CF-31.003.402.40240
CF-41.023.452.43238
CF-51.013.432.43241
Mean value1.003.412.40239