Effects of Calcination on the Crystallography and Nonbiogenic Aragonite Formation of Ark Clam Shell under Ambient Condition
Figure 3
PXRD patterns of ACS after calcination at 600–1000°C for 3 hours and cooling down with −10°C min−1 under ambient condition (C = calcite; O = fcc CaO).