Research Article

Properties of Calcium Acetate Manufactured with Etching Waste Solution and Limestone Sludge as a Cementitious High-Early-Strength Admixture

Table 5

Measurements and methods.

ExperimentMeasurement sampleProperties measuredStandards

Calcium acetate using limestone sludge and recycled acetateCalcium acetateViscosity (cps)ASTM D 2196 [28]
Density (kg/m3)ASTM D 4052-11 [29]
pH
ICP-MS analysisASTM D 6800-12 [30]

Cement matrix using acceleratorCement pasteSetting timeASTM C 191 [31]
pH
XRD
Cement mortarFlowASTM C 230/230M-14 [32]
Compressive strengthASTM C 109 [33]