Research Article
Influence of Freeze-Thaw Damage on the Steel Corrosion and Bond-Slip Behavior in the Reinforced Concrete
Table 1
Mixture proportions of concrete, Kg/m3.
| Specimen | Cement | Sand | Gravel | Water | Air entrained agent | Silane gel |
| Ordinary concrete | C-0.4 | 380 | 580 | 1270 | 152 | | | C-0.6 | 300 | 699 | 1191 | 180 | | | Air entrained concrete | C-0.6A | 300 | 699 | 1191 | 180 | 0.003% | | Waterproofing concrete | C-0.6W | 300 | 699 | 1191 | 180 | | 400 g/m3 |
|
|