Research Article
Microstructure and Mechanical Behavior of Hot Pressed Cu-Sn Powder Alloys
Table 1
Vickers microhardness values in Kg/mm2 of hot pressed Cu-Sn alloys.
| Alloys | Vickers microhardness () Kg/mm2 | Matrix (-Cu) | Bright (-phase) |
| 90% Cu-10% Sn | 112.2 | 246.6 | 85% Cu-10% Sn-5% C | 83.7 | 162.7 | 80% Cu-10% Sn-10% Pb | 108.9 | 222.2 | 90% Cu-10% Pb | 101.4 | 210.3 |
|
|