Research Article

Investigation on Durability Performance in Early Aged High-Performance Concrete Containing GGBFS and FA

Table 3

Chloride ion penetrability based on charge passed [38].

Charge passed (c)Chloride ion permeability

>4,000High
2,000–4,000Moderate
1,000–2,000Low
100–1,000Very low