Flexural and Shear Behaviors of Reinforced Alkali-Activated Slag Concrete Beams
Table 2
Properties of AAS concrete.
| Fresh concrete | Hardened concrete (28 days) | Slump (mm) | Air content (%) | Compressive strength (MPa) | Elastic modulus (GPa) | Splitting tensile strength (MPa) |
| 165 | 3.1 | 55.3 | 31.5 | 3.9 |
|
|