Improvement of the Early-Age Compressive Strength, Water Permeability, and Sulfuric Acid Resistance of Scoria-Based Mortars/Concrete Using Limestone Filler

Figure 11

Weight losses over time of 28 days’ cured mortars immersed in 5% H2SO4.