Research Article

Improvement of the Early-Age Compressive Strength, Water Permeability, and Sulfuric Acid Resistance of Scoria-Based Mortars/Concrete Using Limestone Filler

Table 2

Mixtures used in the experimental investigation.

Mix typeSample mixture (%)
Clinker + gypsumLimestone filler (LF)Volcanic scoria (VS)

VS0LF010000
VS0LF59550
VS0LF1090100
VS0LF1585150
VS10LF090010
VS10LF585510
VS10LF10801010
VS10LF15751510
VS20LF080020
VS20LF575520
VS20LF10701020
VS20LF15651520
VS30LF070030
VS30LF565530
VS30LF10601030
VS30LF15551530