Research Article
Testing of Microalloyed Steel Quality under Creep Conditions for a New Intended Use
Figure 8
Close to fracture microstructure. (a) C16E after creep exposition at 450°C, 7120 h; (b) H300LAD after creep exposition at 450°C, 8930 h.
(a) |