Research Article

Testing of Microalloyed Steel Quality under Creep Conditions for a New Intended Use

Figure 9

Fracture surface. (a) C16E after creep exposition at 450°C, 7120 h; (b) H300LAD after creep exposition at 450°C, 8930 h.
(a)
(b)