Research Article
Microstructure of Al-Si Slurry Coatings on Austenitic High-Temperature Creep Resisting Cast Steel
Figure 3
Microstructure (BEI) of Al–Si coating on sample (a) number 7 (technological parameters: 800°C, 10 h, Al/Si = 12) and (b) number 2 (technological parameters: 1000°C, 5 h, Al/Si = 6).
(a) |
(b) |