Research Article
Bricks and Concrete Wastes as Coarse and Fine Aggregates in Sustainable Mortars
Figure 9
Visual observation of mortars just after the extraction from the semiimmersion test. In each picture, the specimen on the right was exposed in water, as a reference. (a) M/S1; (b) M/S2; (c) M/S3; (d) M/S1F1; (e) M/S2F2; (f) M/S3F3.
(a) |
(b) |
(c) |
(d) |
(e) |
(f) |