Table 3: Suns- results of an EVA sample measured before and after metallization of the BSF layer using line contacts in combination with an etching step that effectively reduces the shunting between emitter and BSF.

(mV) )pFF (%)

Before metalisation459 Infinity 73.6 1.40
After metalisation455 Infinity 75.7 1.24