Infrared Camera Analysis of Laser Hardening

Figure 11

The enlarged picture of the sample cross-section through the square with parameters 30 kHz and 300 mm/s made by optical microscope Hirox. There are marked depths of regions with changed structure (270 μm) and temperature affected area (816 μm).