Research Article

Fabrication and Evaluation of Large Area Mo/Si Soft X-Ray Multilayer Mirrors at Indus SR Facilities

Figure 8

Measured lateral variation of periodicity along the length obtained from best-fit results of Figure 7.
976868.fig.008