(a)
(b)
(c)
(d)
(e)
Figure 5:
Scanning electron microscopy and scanning Auger electron spectroscopy mapping images for the C KLL, O KLL, Pt MNN, and Ru LMM on Pt-Ru particle deposited sequentially on BDD films using 1.0 mM K
2
PtCl
6
and 1.0 mM RuCl
3
solution.