Review Article

Nanoporous PdCo Catalyst for Microfuel Cells: Electrodeposition and Dealloying

Figure 9

SEM images of nanoporous PdCo dendrites: (a–c) plan view, and (d) cross-sectional. The sample shown in “a” and “b” was electrodeposited at a constant current of –50 mA cm−2 for 600 s followed by the immersion in an air-saturated 0.5 M sulfuric acid solution for ~15 h at 60°C. The sample shown in “c” and “d” was prepared by galvanic pulse deposition and dealloying. Reproduced with permission from [29]. Copyright 2010, Elsevier.
821916.fig.009a
(a)
821916.fig.009b
(b)
821916.fig.009c
(c)
821916.fig.009d
(d)