Research Article
Reinforced, Extruded, Isotropic Magnetic Elastomer Composites: Fabrication and Properties
Table 4
Relative damping values of EOR vulcanizates obtained by various processing methods.
| Sample | Carbonyl iron powder content [phr] | Carbon black content [phr] | Tτw [%] |
| Composites prepared using traditional rubber processing |
| Reference sample | 60 | - | 24.8±0.3 | Carbon black filled sample | 5 | 20.7±0.1 | 10 | 21.2±0.2 | 15 | 21.9±0.1 | 20 | 21.6±0.1 |
| Composites prepared using extrusion process |
| Reference sample | 60 | - | 24.8±0.5 | Carbon black filled sample | 5 | 26.2±0.2 | 10 | 26.8±0.3 | 15 | 26.2±0.1 | 20 | 27.2±0.4 |
|
|