Formation of Composite Surface during Friction Surfacing of Steel with Aluminium
Table 1
Processing parameters for various samples and quality of the deposition.
| Trial no. | Tool travel speed (mm/min) | Load (kN) | Spindle speed (rpm) | Quality of the deposition |
| T1 | 35 | 3 | 200 | Powdery deposition, | T2 | 35 | 3 | 400 | Deposition better than T1, still powdery | T3 | 35 | 4 | 200 | Discontinuous and varying width. | T4 | 35 | 4 | 400 | Good (uniform, continuous) deposition | T5 | 35 | 5 | 200 | Continuous, varying width | T6 | 35 | 5 | 400 | Good deposition, Width more than T4 |
|
|