Research Article

Surface Layer Properties after Successive EDM or EDA and Then Superficial Roto-Peen Machining

Figure 14

Stereometric image of the surface subjected to the: (a) EDM: cooper electrode, I = 32 (A), Ti = 800 (μs); (b) EDA: 1H18N9 electrode, I = 32 (A), Ti = 3200 (μs); (c) EDA + roto peen;  (rev/min),  (s).
723919.fig.0014a
(a)
723919.fig.0014b
(b)
723919.fig.0014c
(c)