Research Article

Correlation between Wear Resistance and Lifetime of Electrical Contacts

Figure 22

(a) Microscopy of contact area (average depth of wear crater: 4 μm, contacts survive a 50,000-cycle test, nanoscale particles modified plating of 0.8 μm). (b) Microscopy of contact area (average depth of wear crater: 6 μm, contacts fail at 50,000-cycle, nanoscale particles modified plating of 0.8 μm).
893145.fig.0022a
(a)
893145.fig.0022b
(b)