Experimental and Theoretical Analysis of Zircaloy-4 and AISI 304 Stainless Steel Material Pair in Water Sliding Conditions

Table 6

Ratio of contact pressure and yield strength for zircaloy-4 and AISI 304 SS.

Applied Load, F
(N)
Contact pressure
(MPa)
54751.242.20
85551.452.58
116161.612.68