Research Article

Dynamic Mechanical Response of Biomedical 316L Stainless Steel as Function of Strain Rate and Temperature

Table 2

Work-hardening rate of various alloys at 25°C.

MetalStrain rate (s−1)True strainWork-hardening rate (MPa/unit strain)Reference

316L stainless steel10000.11500current study
6000 series Al-Sc alloy12000.1403.2[28]
Unweldable Al-Sc alloy12000.1200[26]
Weldable Al-Sc alloy13000.1160[27]
Biomedical Ti alloy8000.1250[25]