Ethanol Postpolymerization Treatment for Improving the Biocompatibility of Acrylic Reline Resins
Table 2
Mean (×104 µg/g) and SD of RM content of experimental groups from material Kooliner () and Ufi Gel Hard ().
Material
Temp.
Dry conditions
Type of solution
Water
Ethanol 20%
Ethanol 50%
Ethanol 70%
Kooliner
23 ± 2°C
2.77 (0.29)aA
2.51 (0.16)aA
2.56 (0.25)aA
2.57 (0.31)aA
2.46 (0.41)aA
55 ± 2°C
2.67 (0.22)aA
2.04 (0.21)bB
1.88 (0.15)bB
1.59 (0.14)cB
0.80 (0.16)dB
Ufi Gel Hard
23 ± 2°C
1.90 (0.15)aA
1.62 (0.26)bA
1.58 (0.17)bA
1.52 (0.23)bA
1.45 (0.11)bA
55 ± 2°C
1.85 (0.32)aA
0.95 (0.05)bB
0.86 (0.42)cB
0.72 (0.13)dB
0.39 (0.05)eB
Horizontally identical superscripted small letters denote no significant differences among groups (). Vertically identical superscripted capital letters denote no significant differences among groups ().