Titanium Surface Coating with a Laminin-Derived Functional Peptide Promotes Bone Cell Adhesion
Table 1
The means and standard deviations of the compositions and roughness for the investigated Ti disc surfaces.
| | c.p. Ti | SLA | Anodized | (Ca-P) coated |
| Compositions (wt %) | | | | | Ti | 104.0 (0.4) | 96.1 (1.0) | 52.7 (2.4) | 61.8 (2.7) | O | 4.1 (0.4) | 3.5 (0.3) | 41.7 (0.6) | 37.2 (1.9) | Ca | | | 5.9 (0.7) | 14.0 (0.5) | P | | | 1.9 (0.3) | 2.2 (0.4) | Roughness parameters | | | | | (m) | 0.65 (0.05) | 1.72 (0.26) | 0.68 (0.02) | 1.74 (0.09) | (%) | 22.2 (2.5) | 102.3 (21.7) | 44.1 (4.3) | 90.6 (9.1) |
|
|