Research Article

Magnesium Coated Bioresorbable Phosphate Glass Fibres: Investigation of the Interface between Fibre and Polyester Matrices

Figure 1

Transverse view of magnesium film deposition onto a glass slide after coating at 30 w for 120 min.
735981.fig.001a
(a)
735981.fig.001b
(b)