Research Article

Fracture Strength of Aged Monolithic and Bilayer Zirconia-Based Crowns

Table 2

Mean fracture strength and Tukey’s test results at 95% significance level.

Experimental groupFracture strength ()Std. deviationTukey ( = .05)

Polished monolithic (PM)3492.5748.21a
Glazed monolithic (GM)3344.71159.45a
Bilayered veneered (BL)2051.8764.76b*

*Statistical difference among experimental groups ( = .002).