Mean yttrium content (wt%) in monolithic crowns and Tukey’s test results at 95% significance level.

Experimental groupYttrium content (wt%)Std. deviationTukey
( = .05)

PM worn occlusal 2.07850.9361a*
GM worn occlusal2.08220.6728a
PM undamaged2.07000.6443a

*Similar letters indicate statistically similar results among all groups ( = .935).