Correspondence between degradation period and stretch ratio ().

Degradation period /Average circumferential stress of intima /MPaAverage circumferential strain of intima /%Stretch ratio/%

00.363 ± 0.00413.1 ± 0.21315
0.30.304 ± 0.00311.7 ± 0.14110
0.60.247 ± 0.0029.6 ± 0.075
0.90.137 ± 0.0025.5 ± 0.0615