Data describing roughness (AFM) results.

Mean (nm)Standard deviationMinimum (nm)Median (nm)Maximum (nm)

C51.3714.087132.7747.1369.827
P194.8933.6454148.17198.42241.56
E135.4513.8431108.7139.3154.1
PE151.029.4608138.2149.7170.2