Research Article

Evaluation of High-Performance Polyether Ether Ketone Polymer Treated with Piranha Solution and Epigallocatechin-3-Gallate Coating

Table 4

Tukey’s test of multiple comparisons for different groups of roughness test results.

Tukey’s HSD test
Group pairsDifferenceStandard error score valueSig.

C vs. P143.52096.34744222.61082< 0.00001S
C vs. E84.07696.34744213.24579< 0.00001S
C vs. PE99.64696.34744215.69875< 0.00001S
P vs. E59.4446.3474429.365032< 0.00001S
P vs. PE43.8746.3474426.9120760.00012S
E vs. PE15.576.3474422.4529570.32128NS