Chemical groups and environments present in the derived structure of Chronoflex PU. The underscored atom shown in the group column is the contributing chemical environment of that row.

Chemical environmentInstancesArea ratioGroupBinding energy (eV)Reference

Carbon
 12121/32C–C285.0[6, 14]
 233/32C–O–C=O286.6[6]
 321/16O=C(–O)–N287.9–289.4[6, 15]
 411/32O=C(–O)–O290.35–290.44[6]
 521/16N–Chex285.5–286.4[6]
 633/32C–O–R286.1–286.75
286.4–286.8
[6]
[14]

Total321

Nitrogen
 111O=C–N–C399.9–400.2[6]

Oxygen
 122/7O–C(=O)–N531.3–532.4[6]
 222/7O–C(=O)–N533.2–533.9
533.5–533.7
[6]
[14]
 311/7C–O–C(=O)–O532.3-532.4
532.0–532.3
[6]
[14]
 422/7O–C(=O)–O533.8–534.0
533.5–533.9
[6]
[14]
 —C–O–H532.8–533.1
532.7–533.1
[6]
[14]

Total71