High Gain and High Directive of Antenna Arrays Utilizing Dielectric Layer on Bismuth Titanate Ceramics

Figure 2

FESEM image of BiT: (a) calcined powder at 750°C for 3 hours and (b) sintered bulk ceramic at 1100°C for 3 hours.